logo
Home ProductsDifferential Scanning Calorimeter

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

Certification
China DONGGUAN LONROY EQUIPMENT CO LTD certification
China DONGGUAN LONROY EQUIPMENT CO LTD certification
I'm Online Chat Now

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC
ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

Large Image :  ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

Product Details:
Place of Origin: Guangdong, China
Brand Name: LONROY
Payment & Shipping Terms:
Minimum Order Quantity: 1

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

Description
Type: Testing Machine Accuracy Class: High Accuracy
Accuracy: ---- Application: Auto Testing, Laboratory Testing, Lab Testing
Customized Support: OEM, ODM, OBM Power: ---
Protection Class: Ip56 Voltage: 220 V
Warranty: 1 Year Overall Dimensions: 800*800*3370mm Or 800*800*3600mm
Total Weight: 390Kg/450Kg
Highlight:

ISO 11357 touchscreen DSC tester

,

laboratory phase transition testing machine

,

oxidation induction tester with warranty

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase Transition Testing Machine

 

Product Introduction

The differential scanning calorimeter is touchscreen-based and can be used for testing the glass transition temperature, phase transition, melting and heat enthalpy, product stability, and oxidation induction period.

 

Compliant with standards

GB/T 19466.2–2004 / ISO 11357-2:1999 - Part 2: Determination of Glass Transition Temperature

GB/T 19466.3–2004 / ISO 11357-3:1999 - Part 3: Determination of Melting and Crystallization Temperatures and Thermal Enthalpy

GB/T 19466.6-2009 / ISO 11357-3:1999 - Part 6: Determination of Oxidation Induction Time and Oxidation Induction Temperature

 

Technical features

1. An industrial-grade 8-inch touch screen with rich display information.

2.USB communication interface, with strong universality, reliable communication without interruption, and supports self-recovery connection function.

3. Unique furnace body sealing performance, which can provide excellent experimental conditions.

4. Automatic switching of two gas flow rates, with fast switching speed and short stabilization time. At the same time, an additional protective gas input is added.

5. Simple and easy-to-use software.

 

 

 

IISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase Transition Testing Machine

 

Technical Specification

 

Temperature range

Room temperature to 500℃

Temperature resolution

0.01℃

Temperature fluctuation

±0.1℃

Temperature repeatability

±0.1℃

Heating rate

0.1 to 100℃/min

Constant temperature time

Recommended < 24 hours

Temperature control method

Heating, constant temperature (fully automatic program control)

DSC range

0 to ±600mW

DSC resolution

0.01mW

DSC sensitivity

0.01mW

Working power supply

AC220V/50Hz or custom

Atmosphere control gas

Nitrogen, Oxygen (instrument automatically switches)

Gas flow rate

0 - 300mL/min

Gas pressure

0.2MPa

Display method

24-bit color, 8-inch LCD touch screen display

Data interface

Standard USB interface

Parameter standard

Equipped with standard substances (indium, tin, zinc), users can calibrate the temperature themselves

 

 
 
 

ISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSCISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSCISO 11357 ISO 11357 Touchscreen Differential Scanning Calorimeter Oxidation Induction Tester Laboratory Phase DSC

Contact Details
DONGGUAN LONROY EQUIPMENT CO LTD

Contact Person: Kaitlyn Wang

Tel: 19376687282

Fax: 86-769-83078748

Send your inquiry directly to us (0 / 3000)