Product Details:
|
| Voltage: | 220V | Protection Class: | Ip56 |
|---|---|---|---|
| Force Resolution: | 0.01 KN | Force Value Accuracy: | ±1% FS |
| Maximum Stretching Displacement: | 550mm, 600mm | Speed: | 0.3mm - 50mm/min |
| Number Of Workstations: | 1 Workstation, 3 Workstations | Model: | Horizontal Type, Vertical Type |
| Loading Method: | Electronic Type, Mechanical Type | Measuring Range: | 0 - 50 KN, 0 - 20 KN |
| Displacement Accuracy: | 0.03mm, 0.02mm | Temperature Control: | -30 To 70℃; Customizable |
| Force Range: | 0 - 50 KN, 0 - 20 KN | Displacement Range: | 550mm, 600mm |
| Speed Range: | 0.3mm - 50mm/min | ||
| Highlight: | Geosynthetic material creep tester 50kN,Textile testing machine 600mm displacement,Creep test system with warranty |
||
| Parameter | Specification |
|---|---|
| Number of Workstations | 1 workstation, 3 workstations |
| Model | Horizontal type, Vertical type |
| Loading Method | Electronic type, Mechanical type |
| Measuring Range | 0 - 50 kN, 0 - 20 kN |
| Force Resolution | 0.01 kN |
| Force Value Accuracy | ±1% FS |
| Maximum Stretching Displacement | 550mm, 600mm |
| Displacement Accuracy | 0.03mm, 0.02mm |
| Speed | 0.3mm - 50mm/min |
| Temperature Control (Optional) | -30 to 70℃; Customizable |